By:Bill Hamm
Date: 8/15/2011, 4:00 pm

: One part poly ... you're best off with oil based exterior grade
: slow dry poly ... ZAR works well but there are others. Depending
: on where you are oil based anything may be very tough to find
: these days.

: Ken Blanton

Hi Ken,

We locally can't buy oil based house paint anymore, but oil based varnish is in all the stores. Odd.

Bill H.

Messages In This Thread

Skin-on-Frame: Polyester resin to dope skin-on-frame
Luke Hospadaruk -- 8/15/2011, 2:21 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Bill Hamm -- 8/15/2011, 2:32 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Luke Hospadaruk -- 8/15/2011, 3:07 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
StephenHJ -- 8/15/2011, 3:29 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Ken Blanton -- 8/15/2011, 3:40 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Bill Hamm -- 8/15/2011, 4:00 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Bill Hamm -- 8/15/2011, 4:03 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Bill Hamm -- 8/15/2011, 2:33 pm
Re: Skin-on-Frame: Polyester resin to dope skin-on
Brian Nystrom -- 8/16/2011, 6:43 am
Re: Skin-on-Frame: Polyester resin to dope skin-on
Mike Savage -- 8/16/2011, 9:22 am