Re: Skin-on-Frame: Frame finishing
By:Brian Nystrom
Date: 5/17/2014, 9:42 am
In Response To: Skin-on-Frame: Frame finishing (Jack Hawkins)

Tung oil will work just fine. Brush it on, then go back and wipe off any excess. After 24 hours at room temperature, it should be ready for skinning. FWIW, I've never had an issue with oil bleeding through the skin on my boats, but I don't leave excess finish on the frame, either.

Messages In This Thread

Skin-on-Frame: Frame finishing
Jack Hawkins -- 5/16/2014, 8:37 am
Re: Skin-on-Frame: Frame finishing
Mike Bielski -- 5/16/2014, 10:40 am
Re: Skin-on-Frame: Frame finishing
Jack Hawkins -- 5/16/2014, 9:07 pm
Re: Skin-on-Frame: Frame finishing
Marc Upchurch -- 5/16/2014, 12:07 pm
Re: Skin-on-Frame: Frame finishing
Jack Hawkins -- 5/16/2014, 9:01 pm
Re: Skin-on-Frame: Frame finishing
Brian Nystrom -- 5/17/2014, 9:42 am
Re: Skin-on-Frame: Frame finishing
Dave Gentry -- 5/18/2014, 10:12 pm