Re: Material: WEST SYSTEM 206
By:Sam McFadden
Date: 9/17/2009, 5:41 pm
In Response To: Material: WEST SYSTEM 206 (Scott Fitzgerrell)

Scott,

If you feel there was blush on the surface prior to recoating, make sure you sand through the topcoat and wash the sanded surface well with water and a scrub pad - or wet sand.

Washing is a good practice with all epoxy brands since "no blush" really means low blush.

Sam

: Had to use some of this stuff in an emergency. Lot of blush, which I didn't
: see before recoating. What do I do, sand it down a bit and then recoat?
: I'm used to nonblushing epoxies, mostly Raka, and was not alert to this
: problem. I'm thinking of just sanding down with 120/180 grit and recoating
: with Raka. Problems?

: --S

Messages In This Thread

Material: WEST SYSTEM 206
Scott Fitzgerrell -- 9/16/2009, 8:14 pm
Call West
Jay Babina -- 9/17/2009, 7:13 pm
Re: Call West
Scott Fitzgerrell -- 9/18/2009, 1:43 am
Re: Call West
Bill Hamm -- 9/19/2009, 8:15 am
Re: Material: WEST SYSTEM 206
Sam McFadden -- 9/17/2009, 5:41 pm