I used doug fir for my gunwhales, keelson, and stringer. The ribs and coaming are made of clear white pine. All of it was kiln dried, so for bending the ribs and coaming stock were soaked in a length of 4" pvc pipe filled with water for a minimum of 24 hours. No breakage occurred.

This winter I'm gonna do SOF canoe and the ribs will kiln dried oak.
Randy

Messages In This Thread

Skin-on-Frame: Wood
Kellan Hatch -- 9/24/2002, 3:48 pm
Re: Sitka Spruce
Jay Babina -- 9/26/2002, 10:07 am
Re: Sitka Spruce
Rehd -- 9/26/2002, 10:55 am
Re: Skin-on-Frame: Wood *Pic*
Roger Nuffer -- 9/25/2002, 6:50 pm
Re: Skin-on-Frame: Wood
West -- 9/25/2002, 9:00 pm
Re: Skin-on-Frame: Wood
Roger Nuffer -- 9/25/2002, 10:28 pm
Re: Skin-on-Frame: Wood
Randy -- 9/25/2002, 9:31 am
Re: Skin-on-Frame: Wood
Tony -- 9/24/2002, 4:41 pm
Re: Skin-on-Frame: Wood
Brian Nystrom -- 9/24/2002, 4:18 pm